DUPONT DELRIN 510MP POM Resin
DUPONT Delrin 510MP is a POM by DuPont, with 10% Teflon micropowder for low friction and wear in various industries.
Physical Properties
- Density: Determined by the ASTM D792 standard, it is 1.48 g/cc (0.0535 lb/in³), useful for comparing with other materials in terms of density.
- Linear Mold Shrinkage: At 3.20 mm thickness, it ranges from 0.017 – 0.020 cm/cm in 24 hr (ASTM D955), affecting the accuracy of molded parts.
- Linear Mold Shrinkage, Transverse: At 3.20 mm thickness, it ranges from 0.017 – 0.020 cm/cm in 24 hr (ASTM D792), which is important for the transverse dimensional accuracy of products.
- Melt Flow: At 190°C with a 1.05 kg load, it is 5.0 g/10 min (ASTM D1238), reflecting its melt – state flow characteristics.
Polymer Properties:
- Base Material: Polyoxymethylene (POM)
- Modification Features
- 10% Teflon® PTFE micropowder reduces friction.
- Enhances wear resistance of the base resin.
- Maintains good mechanical property balance.
Applications:
The combination of enhanced toughness, good mechanical properties, and excellent processability makes Delrin 510MP a versatile material for a wide range of durable and demanding applications.
- Automotive Components: Ideal for interior and under-the-hood parts that need to be both strong and impact-resistant, such as gearshift levers, seat components, and snap-fit assemblies.
- Industrial Components: Used for robust parts in machinery, power tool casings, and conveyor systems that are prone to accidental drops or impacts.
- Consumer Goods and Toys: Suitable for durable, moving parts in appliances, toys, and sports equipment that are subject to frequent use and rough handling.
- Precision Engineering: Employed in precision gears and mechanical linkages where a balance of strength and toughness is required.